When a toy fails a chemical test, the finding usually points at the surface. Pigments, driers, some stabilisers and a handful of legacy additives are where the regulated elements enter a toy, which is why the coated and painted part is the sample the laboratory most often scrapes. The failure is rarely dramatic: the product looks perfect, passes every mechanical test, and then returns a migration result a few milligrams over the limit.
Understanding why that happens starts with the type of limit. Modern toy standards do not limit how much of an element is present; they limit how much comes out of the material under conditions chosen to simulate a child swallowing it. That single distinction explains most of the confusion between a screening result that looks alarming and a compliance result that passes.

Migration, Not Content
The European and American toy standards both work on migration, and the structure is worth knowing before reading any report:
- Material categories: the European standard divides materials into dry, brittle or powdery substances such as chalk and clay; liquid or sticky substances; and scraped-off coatings, plastics and similar materials. Each has its own limits.
- Listed elements: the regulated list covers among others lead, cadmium, chromium, mercury, arsenic, selenium, barium and antimony, each with its own limit per category.
- Simulated extraction: the sample is extracted under conditions modelled on stomach contact, and the amount released is measured, not the amount contained.
- Total limits: surface coatings on toys also carry total content limits for lead and, in the American rules, for a small list of other elements, which are separate from the migration figures.
The practical effect is that a paint with a measurable lead content can still pass if the element is locked into the film, while a nominally low-content paint can fail if the film releases it. Neither outcome can be predicted from the tin.

Screening, Testing and Knowing the Difference
Handheld XRF screening is the most useful tool a buyer can put on this problem, and the most commonly misused. It measures total element content in seconds, without preparing a sample, which makes it excellent for sorting incoming paint lots, checking a returned batch and triaging a warehouse before a formal test. It is not a compliance result. A screening pass does not satisfy a standard, and a screening hit is an instruction to send a sample to the laboratory, not evidence of failure.
The compliance result comes from the accredited laboratory, which scrapes or prepares the sample, runs the extraction and reports migration by element. A sensible buying policy uses both: screening on every incoming paint or pigment lot as a cheap control, and formal migration testing on the finished part at the frequency the market requires, with any screening hit escalated immediately rather than averaged away.
Why a Compliant Paint Stops Complying
Three changes account for most surprises on an established line. A pigment is substituted, often for a brighter colour or a lower price, and the replacement carries an element the original did not. A thinner, hardener or catalyst is changed, which alters the cured film and therefore its release behaviour even when the pigment is unchanged. And the film itself changes: a thicker spray, a shorter cure or a lower oven temperature leaves a coating that releases more than the one that was tested.
Each of those is a process variable, which means the control belongs on the paint line rather than in the laboratory calendar. State the paint supplier and grade, the thinner and mixing ratio, the applied film thickness range and the cure time and temperature, and hold a retained sample per batch. When a result comes back high, those four records tell you where the change happened within minutes.

Технический контекст
The historical source of the concern is lead paint, whose use in consumer goods is what the modern limits were written to end. Among the regulated elements, cadmium is the one most often carried by bright pigments, and the screening instrument used to sort them is X-ray fluorescence, which reads total content rather than migration.
Specifying Coatings for a Bulk Run
The specification that holds a paint line steady has five lines: the paint supplier and product code, the pigment list with any element declaration, the thinner and mixing ratio, the applied thickness and cure parameters, and the retained sample per batch. Add the inspection method – an XRF screen on incoming lots and on finished parts at an agreed frequency – and the frequency of formal migration testing, which is typically annual for a stable line and immediate after any material change.
Unpainted does not mean untested. Bare wood, anodised metal and printed paper surfaces all sit in the scope of the standards, and a printed carton label on a toy is as much an accessible surface as a painted one. The material choice should be made once, on the bill of materials, and every subsequent substitute should be treated as a change requiring evidence.
The wider certification scope around these limits is set out in руководстве по сертификации EN71, ASTM и CPC, and the laboratory cost and timing in путеводителе по бюджету и срокам тестирования игрушек. Wooden products carrying these coatings are treated in путеводителе по классам материалов для деревянных игрушек, and holding the finish consistent across a run follows the colour consistency guide.
Частые вопросы
Is the limit on total content or on migration?
On migration, which measures how much of the element is released under simulated stomach contact. Total limits exist for coatings but are a separate requirement.
Which elements are covered?
The regulated list includes lead, cadmium, chromium, mercury, arsenic, selenium, barium and antimony, each with a limit that depends on the material category.
What materials are tested?
Dry brittle or powdery materials, liquid or sticky materials, and scraped-off coatings and plastics, each treated as a separate category with its own limits.
Can XRF screening replace laboratory testing?
No. It screens total content in seconds and tells you where to look; the compliance result comes from the accredited laboratory migration test.
What makes one batch pass and the next fail?
A substituted pigment, a changed thinner or hardener, or a film thickness and cure that differ from the one that was tested.
Is a paint supplier’s certificate enough?
No. The finished coated part needs migration testing, because the substrate, thinner and cure all affect what the film releases.
How often should coatings be retested?
At least annually on a stable line, and immediately after any change to the paint, pigment lot, thinner or cure process.